Item | Corundum High-Strength Castable | Sic Surface Crusting Resistant Castable | High Strength And Speed-Setting Castable | |||||
HWG-16 | HWG-17 | HWG-18 | HWK-50 | HWK-55 | HWPA80 | HWPAF80 | ||
AI2O3(%) ≥ | 85 | 90 | 93 | 80 | 80 | |||
SiO2(%)≤ | 10 | 6 | 2 | |||||
SiC(%)≤ | ||||||||
B.D g/cm3≥ | 2.9 | |||||||
C.C.S.(MPa)≥ | 110℃x24h | 80 | 100 | 80 | 70 | 70 | 50 | 70 |
1100℃x3h | 80 | 100 | 80 | 80 | 80 | 60 | 80 | |
1500℃x3h | 80 | 100 | 80 | |||||
M.O.R MPa≥ | 110℃x24h | 8 | 12 | 8 | 8 | 8 | 7 | 8 |
1100℃x3h | 8 | 12 | 8 | 7 | 7 | 8 | 10 | |
1500℃x3h | 8 | 12 | 8 | |||||
P.L.C(%) | 1100℃x3h | -0.10~-0.30 | -0.10~-0.30 | ±0.2 | ±0.3 | ±0.4 | ±0.4 | -0.20~-0.50 |
1500℃x3h | -0.10~-0.50 | -0.20~-0.60 | ±0.5 | |||||
Maximum Service Temperature ℃ | 1650 | 1700 | 1750 | 1300 | 1400 | 1500 | 1500 | |
Installation Method | Vibration | Vibration | Vibration | Vibration | Vibration | Ramming | Ramming | |
Water Required(%) | 5~6 | 5.5~6.5 | 5.5~6.5 | 6~7 | 6~7 | |||
Main Use | Entrance, Coal Spraying Pipe | Entrance, Coal Spraying Pipe | Entrance, Coal Spraying Pipe | Cone Of Preheater, Up-Take Gas Duct, Inclined Track | Entrance, Repairing Of Cooling Machine | Entrance, Repairing Of Cooling Machine |